vol149cer

FINE GROUND SODIUM HECTORITE

OxideAnalysisFormula
CaO0.65%0.095
MgO2.67%0.540
K2O0.31%0.027
Na2O2.57%0.338
TiO20.16%0.016
Al2O321.08%1.686
SiO263.02%8.554
Fe2O33.25%0.166
LOI6.30
Oxide Weight764.47
Formula Weight815.87
If this formula is not unified correctly please contact us.

A standard viscosity sodium bentonite with an average particle size ranging between 200 and 325 mesh. It is a general purpose suspending and binding agent, economical for brick and refractory manufacturers.

Specific Gravity: 2.5
pH (5% dispersion): 8.5-10.5
C.E.C. (meq/100g): 92
Dry Brightness (Green Filter): 60
Color: Gray
% Moisture Content: 12% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 170cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol149cer" descrip="FINE GROUND SODIUM HECTORITE" searchkey="" loi="6.30" casnumber="12173-47-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.650" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.670" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.310" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.570" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.160" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.080" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.020" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.250" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="6.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved