COLLOIDAL MAGNESIUM SILICATE

OxideAnalysisFormula
CaO2.78%0.133
MgO11.40%0.757
K2O0.96%0.027
Na2O1.92%0.083
TiO20.17%0.006
Al2O39.77%0.256
SiO268.10%3.033
Fe2O31.39%0.023
LOI3.50
Oxide Weight258.28
Formula Weight267.64
If this formula is not unified correctly please contact us.

A highly refined, inorganic complex colloidal, magnesium aluminum silicate. Used as a plasticizing agent in sanitary ware to improve green strength in prefired bodies.

Specific Gravity: 2.5
pH (5% dispersion): 9.5-10.5
C.E.C. (meq/100g): 90
Dry Brightness (Green Filter): 80
Color: White
% Moisture Content: 10% Max.
Brookfield Viscosity (60 rpm @ 5% solids): 3310cps


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="vol105cer" descrip="COLLOIDAL MAGNESIUM SILICATE" searchkey="" loi="3.50" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.780" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="11.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.960" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.920" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.170" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.770" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.390" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="3.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved