1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Virginia Kyanite

Oxide Analysis Formula
SiO2 37.46% 1.06
Fe2O3 0.91% 0.01
Al2O3 59.90% 1.00
TiO2 0.92% 0.02
Na2O 0.20% 0.01
K2O 0.20% 0.00
MgO 0.06% 0.00
CaO 0.05% 0.00
LOI0.29%
Oxide Weight 169.77
Formula Weight 170.27

Related Information

Links

Materials Mullite
Materials Pyrophyllite
Materials Kyanite
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved