Vanadium Pentoxide

Formula: V2O5
Alternate Names: Vanadium (V) Oxide

OxideAnalysisFormula
V2O5100.00%1.000
Oxide Weight181.90
Formula Weight181.90
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.40
GSPT - Frit Softening Point 690C M

A coloring agent that produces yellows, especially when in combination with tin oxide. It is also a strong flux.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Vanadium Pentoxide" descrip="" searchkey="Vanadium (V) Oxide" loi="0.00" casnumber="87854-56-6"> <oxides> <oxide symbol="V2O5" name="Vanadium Pentoxide" status="" percent="100.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved