Alkali-Zink-Bor

Alternate Names: V 15098,V-15098

OxideAnalysisFormula
CaO0.28%0.411
K2O0.35%0.306
ZnO0.28%0.283
B2O30.16%0.189
SiO23.16%4.329
Oxide Weight348.25
Formula Weight348.25
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 70
GSPT - Frit Softening Point 655C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="V15098" descrip="Alkali-Zink-Bor" searchkey="V 15098,V-15098" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.280" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.350" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.280" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="0.160" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="3.160" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved