UGS Spodumene

Spodumene Concentrate

OxideAnalysisFormula
CaO0.40%0.029
Li2O6.10%0.833
MgO0.20%0.020
K2O1.00%0.043
Na2O1.00%0.066
P2O50.30%0.009
TiO20.20%0.010
Al2O322.00%0.878
SiO268.00%4.606
Fe2O30.40%0.010
MnO0.20%0.011
H2O0.30
Oxide Weight406.27
Formula Weight407.49
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.2
HMOH - Hardness (Moh) 6-5-7
SADR - Sieve Analysis Dry -5600 +4000 microns: 2% -4000 +2000: 14% -2000 +1000: 19 -1000: 65
GSPT - Frit Softening Point 1420C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="UGS Spodumene" descrip="Spodumene Concentrate" searchkey="" loi="0.00" casnumber="66057-55-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.400" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="6.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.300" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.200" tolerance=""/> </oxides> <volatiles> <volatile symbol="H2O" name="Water" percent="0.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved