Toyama Feldspar

OxideAnalysisFormula
CaO0.13%0.014
MgO0.35%0.051
K2O4.95%0.308
Na2O0.40%0.038
P2O50.03%0.001
TiO20.15%0.011
Al2O317.38%1.000
SiO269.02%6.740
Fe2O32.97%0.109
MnO0.02%0.002
LOI4.60
Oxide Weight559.88
Formula Weight586.88
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Toyama Feldspar" descrip="" searchkey="" loi="4.60" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.130" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.350" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.950" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.400" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.030" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.150" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.380" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.020" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.970" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.020" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="4.600" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved