Torrecid Frit MBK00020

Calcium zinc zircon zero boron frit

OxideAnalysisFormula
CaO12.46%0.569
MgO2.12%0.135
K2O2.69%0.073
Na2O2.08%0.086
ZnO4.38%0.138
TiO21.39%0.045
Al2O318.56%0.466
SiO246.56%1.983
Fe2O30.13%0.002
ZrO29.50%0.197
LOI3.34
Oxide Weight255.67
Formula Weight264.50
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Torrecid Frit MBK00020" descrip="Calcium zinc zircon zero boron frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.460" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.120" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.690" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.080" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="4.380" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.390" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.560" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.560" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.130" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.500" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="3.340" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved