Torrecid Frit MBK00007

Zinc calcia magnesia titania low-alumina zero-boron frit

OxideAnalysisFormula
CaO12.74%0.448
MgO4.03%0.197
K2O2.68%0.056
Na2O0.30%0.010
ZnO11.96%0.290
TiO25.40%0.133
Al2O33.03%0.059
SiO254.12%1.775
Fe2O30.15%0.002
ZrO24.30%0.069
SO41.29
Oxide Weight194.57
Formula Weight197.12
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Torrecid Frit MBK00007" descrip="Zinc calcia magnesia titania low-alumina zero-boron frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.740" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.030" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.680" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="11.960" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="5.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.030" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.120" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.150" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="4.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="1.290" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved