Torrecid Frit 31056

High zinc opacified frit

OxideAnalysisFormula
CaO11.19%0.454
MgO2.11%0.119
K2O5.26%0.127
Na2O0.21%0.008
ZnO10.48%0.293
TiO20.08%0.002
Al2O36.89%0.154
SiO255.06%2.083
Fe2O30.11%0.002
ZrO27.55%0.139
LOI0.99
Oxide Weight224.97
Formula Weight227.22
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Torrecid Frit 31056" descrip="High zinc opacified frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.190" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.110" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.260" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.210" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.480" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.080" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.890" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.060" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.110" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="7.550" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.990" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved