Tincar

Used in South America

OxideAnalysisFormula
CaO0.42%0.035
MgO0.30%0.034
K2O0.53%0.026
Na2O0.06%0.004
TiO20.49%0.028
Al2O322.10%1.000
SiO263.50%4.876
Fe2O30.60%0.017
LOI12.00
Oxide Weight406.15
Formula Weight461.54
If this formula is not unified correctly please contact us.

We do not know alot about this material, apparently it appears in recipes from South America. We have arbitrarily estimating an LOI based on the analysis.
In one glaze recipe we saw, these were no other clays, so this is probably a clay. It has very low flux content, so it is likely refractory. It has an LOI like a kaolin, but the chemistry is more like a ball clay. So to substitute for it you could try 50:50 kaolin:ball clay.



By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Tincar" descrip="Used in South America" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.420" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.530" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.060" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.490" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="12.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved