Tile #6 Kaolin

Highly Plastic Fine Grained

Alternate Names: Tile 6, Tile#6 Kaolin, #6 Tile kaolin

OxideAnalysisFormula
CaO0.30%0.014
MgO0.40%0.027
Na2O0.10%0.004
TiO21.40%0.047
Al2O338.10%1.000
SiO245.50%2.027
Fe2O30.50%0.008
LOI13.50
Oxide Weight231.04
Formula Weight267.10
If this formula is not unified correctly please contact us.

6 Tile is an airfloated kaolin with bright firing properties yet highly plastic. It thus offers high green strength for superior jiggering and wet processing properties.

Particle size, % < 2 microns 60
325 mesh screen residue, % max 0.5
M.B.I. (meq/100g) 9.8
Specific Surface Area (sq-m/g) 20.0
pH, 20% solids 6.5
*The information given here is from their data sheet dated Jan 2013


Tile #6 Kaolin is the most plastic kaolin available in North America

Tile #6 Kaolin is the most plastic kaolin available in North America

It is a designer kaolin, they add bentonite to the material during manufacture. This vase is made from the pure material, it is very thin and light. The fired color is lighter than what you get when you add common raw bentonite to other less plastic kaolins (to bring them to the same degree of plasticity).

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Tile #6 Kaolin" descrip="Highly Plastic Fine Grained" searchkey="Tile 6, Tile#6 Kaolin, #6 Tile kaolin" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="38.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.500" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="13.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved