TI-21 Ball Clay

Alternate Names: Hick TI-21, Old Hickory TI-21 Ball Clay

Oxide Analysis Formula
CaO 0.07% 0.00
K2O 0.05% 0.00
MgO 0.20% 0.02
Na2O 0.09% 0.01
TiO2 1.58% 0.07
Al2O3 27.30% 1.00
SiO2 58.75% 3.65
Fe2O3 1.00% 0.02
LOI10.90%
Oxide Weight 332.68
Formula Weight 373.37

Notes

Crude Color: Light Grey
Dry M.O.R. (psi 50% clay/50% flint, cast bars): 461
Wet Sieve Residue, +200 mesh (%): 0.51
Water of Plasticity (%): 35
Linear Dry Shrinkage (%): 6.6
Solubles Sulfates (ppm): 199
Filtration (ml): 26
Specific Surface Area (sq meters per gram): 18.1
CEC/MBI (meq/100 ml): 9.5
pH: 6.2
PCE: 31

Firing Shrinkage (%) Cone 04: 5.4 Cone 3: 5.6 Cone 11: 6.6
Absorption (%) 12.8 9.1 3.0

Particle Size (% finer than):
50 microns: 100
20: 97
10: 92
5: 85
1: 60
0.5: 48

Related Information

Links

Materials Ball Clay
Suppliers Old Hickory
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved