Taisyu Feldspar

OxideAnalysisFormula
CaO0.81%0.137
MgO0.03%0.007
K2O0.44%0.044
Na2O5.29%0.811
P2O50.01%0.001
TiO20.11%0.013
Al2O312.29%1.145
SiO280.39%12.709
Fe2O30.03%0.002
MnO0.01%0.001
LOI0.58
Oxide Weight944.54
Formula Weight950.05
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Taisyu Feldspar" descrip="" searchkey="" loi="0.58" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.810" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.030" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.440" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.290" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.110" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.290" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="80.390" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.030" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.010" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.580" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved