Tabular Alumina

Oxide Analysis Formula
Al2O3 100.00% 1.00
Oxide Weight 102.00
Formula Weight 102.00

Notes

Tabular alumina is made by holding calcined alumina powder just below its 2040C fusion temperature to recrystallize the normally flat crystals into hexagonal, elongated tablet-shaped ones up to 400 microns in size. It is possible to convert near 100% of the crystals and achieve a high chemical purity. The new crystals maintain the same hardness and density and have much better thermal shock resistance.

Tabular aluminas are useful in ceramics, electrical insulators, dielectrics and refractory applications. They are available in sizes from around 40 mesh down to 325 mesh.

Related Information

Where to get Tabular Alumina?

Online at Ebay.com apparently!

Links

Materials Alumina Hydrate
Materials Alumina
Materials Calcined Alumina
Suppliers Alcoa
Suppliers High Temp Inc.
Typecodes Alumina
Alumina products

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved