Synthetic Ash

From Ron Roy's MDT

Alternate Names: Synth Ash

OxideAnalysisFormula
CaO50.79%0.895
MgO2.43%0.060
K2O1.60%0.017
Na2O0.49%0.008
P2O52.97%0.021
TiO20.31%0.004
Al2O38.46%0.082
SiO232.62%0.537
Fe2O30.32%0.002
Oxide Weight98.86
Formula Weight98.86
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Synthetic Ash" descrip="From Ron Roy's MDT" searchkey="Synth Ash" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="50.790" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.430" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.490" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="2.970" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.310" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.460" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.620" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.320" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved