OxideAnalysisFormula
CaO0.12%0.014
MgO0.07%0.012
K2O10.16%0.730
Na2O2.23%0.244
Al2O321.31%1.415
SiO262.66%7.059
Fe2O30.25%0.011
LOI3.20
Oxide Weight655.39
Formula Weight677.05
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Stone C" descrip="" searchkey="" loi="3.20" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.120" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.070" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.160" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.230" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.310" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.660" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.250" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="3.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved