Stain 6908

STAIN FLUX (PbBSi)

Old Number: 8
Using stains as underglazes may rob the glaze of its flux causing crawling or dry spots. To alleviate this problem use 10% flux to 90% stain in most situations. For pinks and browns, use a 15:85 ratio.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Stain 6908" descrip="STAIN FLUX (PbBSi)" searchkey="" loi="0.00" casnumber="n/a"> </material>