Stain 6339

Royal Blue (CoAlZn)

Either zircon or tin oxide may be used as an opacifier, zircon being the preferred material.
Underglaze Color: Suitable for use under all types of glazes, firing at temperatures up to over 1300C. Because of their exceptional stability and cleanness of shade, zircon-vandium turquoise blues find wide applications in all types of underglaze decorations.

Suitable for all types of bodies and slips for firing at temperatures up to 1300C. No tendency to flash or strike even under reducing conditions.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Stain 6339" descrip="Royal Blue (CoAlZn)" searchkey="" loi="0.00" casnumber="n/a"> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved