Stain 14 H 548

Orange (ZrVIn)

Suitable for all types of glaze especially those maturing at higher temperatures e.g. sanitaryware types - excellent stability
Max Firing Temp: over 1400C
For Further Information: C8


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Stain 14 H 548" descrip="Orange (ZrVIn)" searchkey="" loi="0.00" casnumber="n/a"> </material>