SP-G Feldspar

Sodium/potassium/calcium Feldspar

OxideAnalysisFormula
CaO1.40%0.140
K2O4.10%0.244
Na2O6.82%0.616
Al2O318.92%1.039
SiO268.15%6.353
Fe2O30.06%0.002
LOI0.08
Oxide Weight557.21
Formula Weight557.65
If this formula is not unified correctly please contact us.
BDLB - Bulk Density lbs/cu. ft. (Packed) 80

Used as an alumina source in glass batch formulations. Beneficiated using the froth flotation process for low iron oxide content.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="SP-G Feldspar" descrip="Sodium/potassium/calcium Feldspar" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.820" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.920" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.150" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.060" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.080" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved