Solargil Frit FR9

Zircon frit

OxideAnalysisFormula
CaO6.09%0.320
K2O5.11%0.160
Na2O5.05%0.240
ZnO7.73%0.280
Al2O313.15%0.380
B2O38.03%0.340
SiO246.48%2.280
ZrO8.36%0.230
Oxide Weight294.80
Formula Weight294.80
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 68.6 x 10-7 C (Appen)
GSPT - Frit Softening Point 940-980C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR9" descrip="Zircon frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.090" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.110" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.050" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.730" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.150" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.030" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.480" tolerance=""/> <oxide symbol="ZrO" name="Zirconium Oxide, Zirconia" status="" percent="8.360" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved