Solargil Frit FR8

Calcium borate frit

OxideAnalysisFormula
CaO17.97%0.680
K2O4.88%0.110
Na2O6.13%0.210
Al2O31.45%0.030
B2O320.01%0.610
SiO249.56%1.751
Oxide Weight212.32
Formula Weight212.32
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 84.9 x 10-7 C (Appen)
GSPT - Frit Softening Point 920-1000C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR8" descrip="Calcium borate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="17.970" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.880" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.130" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.450" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.010" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.560" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved