Solargil Frit FR6

Lead barium boron frit

OxideAnalysisFormula
BaO2.16%0.050
CaO0.95%0.060
K2O5.04%0.190
Na2O5.07%0.290
PbO25.79%0.410
Al2O310.92%0.380
B2O35.10%0.260
SiO243.18%2.549
Fe2O31.80%0.040
Oxide Weight354.84
Formula Weight354.84
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 89.5 x 10-7 C (Appen)
GSPT - Frit Softening Point 940-980C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR6" descrip="Lead barium boron frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.160" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.950" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.070" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="25.790" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.920" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.180" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved