Solargil Frit FR5

High zinc, zero-alumina frit

OxideAnalysisFormula
MgO4.87%0.168
K2O14.06%0.208
Na2O7.49%0.168
ZnO26.61%0.455
SiO246.98%1.089
Oxide Weight139.33
Formula Weight139.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 113.6 x 10-7 C (Appen)
GSPT - Frit Softening Point 1000-1300C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR5" descrip="High zinc, zero-alumina frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.870" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="14.060" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.490" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="26.610" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.980" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved