Solargil Frit FR4

Low alumina very high alkali frit

OxideAnalysisFormula
CaO7.75%0.300
K2O13.01%0.300
Na2O11.42%0.400
Al2O31.41%0.030
SiO266.41%2.400
Oxide Weight217.18
Formula Weight217.18
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 122.4 x 10-7 C (Appen)
GSPT - Frit Softening Point 1000-1300C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR4" descrip="Low alumina very high alkali frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.750" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="13.010" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.420" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.410" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved