Solargil Frit FR3

Calcium borate frit

OxideAnalysisFormula
CaO6.32%0.500
K2O5.31%0.250
Na2O3.49%0.250
Al2O310.34%0.450
B2O321.97%1.401
SiO252.56%3.881
Oxide Weight443.78
Formula Weight443.78
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 61.5 x 10-7 C (Appen)
GSPT - Frit Softening Point 980-1020C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR3" descrip="Calcium borate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.320" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.310" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.490" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.340" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="21.970" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.560" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved