Solargil Frit FR2

Lead bisilicate frit

OxideAnalysisFormula
PbO59.96%1.000
SiO240.03%2.479
Oxide Weight372.21
Formula Weight372.21
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 61.4 x 10-7 C (Appen)
GSPT - Frit Softening Point 950-1000C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR2" descrip="Lead bisilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="59.966" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.034" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved