Solargil Frit FR11

Barium frit

OxideAnalysisFormula
BaO4.95%0.270
CaO4.83%0.720
K2O0.11%0.010
Al2O311.70%0.959
B2O322.04%2.649
SiO256.37%7.845
Oxide Weight836.44
Formula Weight836.44
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Solargil Frit FR11" descrip="Barium frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.950" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.830" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.110" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="22.040" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.370" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved