Oxide Analysis Formula
CaO 41.10% 0.67
K2O 10.96% 0.11
MgO 8.21% 0.19
Na2O 0.77% 0.01
P2O5 4.67% 0.03
SiO2 2.00% 0.03
Fe2O3 0.07% 0.00
MnO 2.54% 0.03
LOI23.00%
SO36.69%
Oxide Weight 64.04
Formula Weight 91.09

Related Information

Links

Materials Cherry Ash
Materials Pine Wood Ash
Materials Wood Ash
Materials Applewood Ash
Materials Oakwood Ash
Materials Eucalyptus Ash
Materials Hardwood Ash
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture

Please check recaptcha to proceed



https://digitalfire.com, All Rights Reserved
Privacy Policy