Sodium Nitrate

A source of sodium in the glass industry

Formula: NaNO3
Alternate Names: Chile Saltpeter, Soda Niter

OxideAnalysisFormula
Na2O36.47%1.000
LOI63.53
Oxide Weight62.00
Formula Weight170.00
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.27
GSPT - Frit Softening Point 310C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Sodium Nitrate" descrip="A source of sodium in the glass industry" searchkey="Chile Saltpeter, Soda Niter" loi="0.00" casnumber="7757-79-1"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="36.470" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="63.530" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved