Sodium Carbonate Heptahydrate

A source of sodium in the glass industry

Formula: Na2CO3.7H2O

OxideAnalysisFormula
Na2O26.72%1.000
CO218.96
H2O54.30
Oxide Weight62.00
Formula Weight231.86
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Sodium Carbonate Heptahydrate" descrip="A source of sodium in the glass industry" searchkey="" loi="0.00" casnumber="3313-92-6"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="26.720" tolerance=""/> </oxides> <volatiles> <volatile symbol="CO2" name="Carbon Dioxide" percent="18.960" tolerance=""/> <volatile symbol="H2O" name="Water" percent="54.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved