Soda Feldspar Z-507-P2

OxideAnalysisFormula
CaO0.97%0.094
MgO0.26%0.035
K2O0.16%0.009
Na2O9.83%0.862
TiO20.03%0.002
Al2O319.57%1.043
SiO268.68%6.211
Fe2O30.07%0.002
LOI0.43
Oxide Weight541.17
Formula Weight543.51
If this formula is not unified correctly please contact us.

A New Zealand material.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Soda Feldspar Z-507-P2" descrip="" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.970" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.260" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.160" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="9.830" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.030" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="19.570" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.680" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.430" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved