Soda-Silica Eutectic 2

OxideAnalysisFormula
Na2O18.40%1.000
SiO281.60%4.575
Oxide Weight336.96
Formula Weight336.96
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 860C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Soda-Silica Eutectic 2" descrip="" searchkey="" loi="0.00" casnumber="n/a"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="18.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="81.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved