Silver Nitrate

Formula: AgNO3
Alternate Names: AgNO3

OxideAnalysisFormula
Ag2O68.22%1.000
LOI31.78
Oxide Weight231.74
Formula Weight339.69
If this formula is not unified correctly please contact us.

Silver nitrate is highly soluble and forms Ag+ ions when dissolved in water. This ion transfers to ware as adhered material and when fired and reduced the Ag metal gives a gold sheen.

It is possible to dry blend the nitrate and carbonate forms and putting these into a glaze to get a better gold sheen.

100 grams of Carbonate is equivalent to 123 grams Nitrate.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Silver Nitrate" descrip="" searchkey="AgNO3" loi="0.00" casnumber=""> <oxides> <oxide symbol="Ag2O" name="Silver Oxide" status="" percent="68.220" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="31.780" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved