Silver Chloride

Formula: AgCl

OxideAnalysisFormula
Ag2O80.82%1.000
Cl24.75
Oxide Weight231.74
Formula Weight307.95
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Silver Chloride" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Ag2O" name="Silver Oxide" status="" percent="80.820" tolerance=""/> </oxides> <volatiles> <volatile symbol="Cl" name="Chlorine Gas" percent="24.750" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved