SicoNide

Silicon Nitride Powder

Purity as little as 0.04 Fe, 0.05 Al, 0.01 Ca, 0.3 C, 0.002 Halides, and 0.7 Oxygen.
Particle sizes available down to 20 microns.

Parmascand, the manufacturer, has a booklet on processing of Si3N4 materials. It covers slip preparation, casing, pressing, tape casting, binders, and sintering.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="SicoNide" descrip="Silicon Nitride Powder" searchkey="" loi="0.00" casnumber=""> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved