SG-328

Albany Slip Substitute

Alternate Names: SG328

Through years of formulation and reformulation, Karl Miller developed Albany Slip Substitute which is intended to reproduce the physical and performance characteristics of the famed Albany (NY) Slip once mined only two hours from Miller's ceramic lab.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="SG-328" descrip="Albany Slip Substitute" searchkey="SG328" loi="0.00" casnumber="70694-09-6"> </material>