SC 1.2 Spodumene

Spodumene Concentrate

OxideAnalysisFormula
CaO0.05%0.003
Li2O7.60%0.979
K2O0.08%0.003
Na2O0.15%0.009
P2O50.17%0.005
TiO20.01%0.000
Al2O326.50%0.998
SiO264.50%4.122
Fe2O30.07%0.002
MnO0.02%0.001
LOI0.20
Oxide Weight380.77
Formula Weight381.54
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 3.2
HMOH - Hardness (Moh) 6-5-7
SADR - Sieve Analysis Dry Tyler 65 mesh: 2% 200 mesh: 62%
GSPT - Frit Softening Point 1420C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="SC 1.2 Spodumene" descrip="Spodumene Concentrate" searchkey="" loi="0.00" casnumber="66057-55-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.050" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="7.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.080" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.150" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.170" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="26.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="64.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.020" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved