SC7.0 Spodumene

Spodumene Concentrate

Alternate Names: Spodumene Concentrate

OxideAnalysisFormula
Li2O7.10%0.968
K2O0.30%0.013
Na2O0.20%0.013
P2O50.20%0.006
Al2O325.50%1.016
SiO264.50%4.361
Fe2O30.13%0.003
LOI0.20
Oxide Weight397.97
Formula Weight398.77
If this formula is not unified correctly please contact us.

Grain size:
+125 mesh - 3% max
-75 mesh - 80% min

As of 2012 this material is being sold as a substitute for Tanco spodumene which is no longer available.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="SC7.0 Spodumene" descrip="Spodumene Concentrate" searchkey="Spodumene Concentrate" loi="0.00" casnumber="66057-55-4"> <oxides> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="7.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="25.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="64.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.130" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved