Sand A

OxideAnalysisFormula
CaO0.09%0.144
MgO0.01%0.022
K2O0.05%0.047
Na2O0.01%0.014
TiO20.11%0.123
Al2O31.14%1.000
SiO298.27%146.299
Fe2O30.07%0.039
LOI0.25
Oxide Weight8925.00
Formula Weight8947.37
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Sand A" descrip="" searchkey="" loi="0.25" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.090" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.010" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.050" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.110" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.140" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="98.270" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.250" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved