Roseville Clay

OxideAnalysisFormula
CaO0.37%0.029
MgO0.21%0.023
K2O2.51%0.116
Na2O0.31%0.022
TiO21.66%0.091
Al2O323.41%1.000
SiO260.89%4.414
Fe2O32.12%0.058
LOI8.51
Oxide Weight398.59
Formula Weight435.66
If this formula is not unified correctly please contact us.
PCE - Pyrometric Cone Equivalent 23

A selectively mined stoneware clay this is exceptionally cean and when ordered in 200 mesh offers the potter a stoneware fireclay which works well by itself or in compound bodies. The fired color is warn buff and it has a firing range of cone 1 to 8. This material will respond to deflocculnts and can thus be used in slip casting bodies.

This has been used for over 100 years by Roseville and Zanesville, OH potters. Some add small amounts of grog to impart texture and improve drying.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Roseville Clay" descrip="" searchkey="" loi="8.51" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.370" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.210" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.510" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.310" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.660" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="23.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.890" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.120" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="8.510" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved