Red Scoria

OxideAnalysisFormula
CaO6.54%0.371
MgO4.12%0.326
K2O3.07%0.104
Na2O3.87%0.199
Al2O321.00%0.656
SiO253.60%2.842
Fe2O36.45%0.128
FeO0.71%0.028
LOI0.65
Oxide Weight316.61
Formula Weight318.69
If this formula is not unified correctly please contact us.

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Red Scoria" descrip="" searchkey="" loi="0.65" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.540" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="4.120" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.070" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.870" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="6.450" tolerance=""/> <oxide symbol="FeO" name="Ferrous Oxide" status="" percent="0.710" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.650" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved