Red Horse Clay

OxideAnalysisFormula
CaO0.45%0.037
MgO0.62%0.071
K2O1.20%0.059
Na2O0.30%0.022
Al2O322.03%1.000
SiO267.59%5.207
Fe2O36.62%0.192
LOI1.18
Oxide Weight457.50
Formula Weight462.96
If this formula is not unified correctly please contact us.

Another analysis show 50% SiO2, 28% Al2O3 and 10% LOI.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Red Horse Clay" descrip="" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.450" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.620" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="22.030" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="67.590" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="6.620" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.180" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved