RCG-5090

OxideAnalysisFormula
CaO0.68%0.119
K2O2.41%0.248
Na2O3.99%0.624
ZnO0.08%0.010
Al2O33.23%0.307
B2O322.29%3.099
SiO267.03%10.793
ZrO20.25%0.020
Oxide Weight967.56
Formula Weight967.56
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="RCG-5090" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.689" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.410" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.997" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.083" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.236" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="22.294" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="67.039" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.252" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved