RCG-3065

OxideAnalysisFormula
CaO12.54%0.654
Li2O0.49%0.048
MgO0.79%0.058
K2O1.23%0.038
Na2O4.28%0.202
Al2O310.39%0.298
B2O36.40%0.269
SiO263.43%3.086
ZrO20.40%0.010
Oxide Weight292.36
Formula Weight292.36
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="RCG-3065" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.544" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.492" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.795" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.239" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.281" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.398" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.408" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.438" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.405" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved