R76 Frit

Alkaline Frit

Alternate Names: R76 Alkalifritte

OxideAnalysisFormula
CaO11.94%0.787
K2O5.43%0.213
Al2O311.81%0.428
B2O317.60%0.935
SiO253.23%3.275
Oxide Weight369.75
Formula Weight369.75
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1000-1200

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="R76 Frit" descrip="Alkaline Frit" searchkey="R76 Alkalifritte" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.940" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.430" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.810" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.230" tolerance=""/> </oxides> </material>