Quartz 762

Alternate Names: Kuvars 762

OxideAnalysisFormula
CaO0.14%0.266
MgO0.15%0.397
K2O0.16%0.181
Na2O0.09%0.155
TiO20.04%0.053
Al2O30.63%0.659
SiO298.60%175.133
Fe2O30.04%0.027
LOI0.15
Oxide Weight10658.90
Formula Weight10674.92
If this formula is not unified correctly please contact us.

Available in -100, -63 and -45 micron sizes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Quartz 762" descrip="" searchkey="Kuvars 762" loi="0.00" casnumber="87347-84-0"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.140" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.150" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.160" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.090" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.630" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="98.600" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.040" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.150" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved