Quartz 761

Alternate Names: Kuvars 761

OxideAnalysisFormula
CaO0.08%0.060
K2O0.16%0.072
Na2O0.27%0.184
Al2O32.41%1.000
SiO296.90%68.239
LOI0.18
Oxide Weight4224.75
Formula Weight4232.37
If this formula is not unified correctly please contact us.

Available in -100, -63 and -45 micron sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Quartz 761" descrip="" searchkey="Kuvars 761" loi="0.00" casnumber="87347-84-0"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.080" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.160" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.270" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="96.900" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.180" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved