Pyrophyl R-2252

Pyrophyllite

OxideAnalysisFormula
K2O0.20%0.008
Na2O0.20%0.013
TiO20.40%0.020
Al2O326.00%1.000
SiO269.70%4.550
Fe2O30.70%0.017
LOI2.80
Oxide Weight381.32
Formula Weight392.31
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.75
SADR - Sieve Analysis Dry +200 mesh: 1%
PCE - Pyrometric Cone Equivalent 29
BDLB - Bulk Density lbs/cu. ft. (Packed) 70

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications. The products have shown to be excellent refractory components in foundry mold and core wash formulations. They also perform in electrical porcelain, technical ceramics and structural clay coatings.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pyrophyl R-2252" descrip="Pyrophyllite" searchkey="" loi="2.80" casnumber="12269-78-2"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="26.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="2.800" tolerance=""/> </volatiles> </material>